According to my brother who is a certed welder the metal was getting to hott and piping while welding and that's why I was getting the popping and funky chasers that would rise out of the weld? When it was turned down I could see good penetration and was getting good lines and they all got 3 good smacks with a 12 pound sledge so their solid.
What seems funny? I have no clue really about welding.
Fat fingered from the phone- Corey
Nothing really bad, just that thee seems to be a lot of carbonizing going on and a bit smokey...Almost like what you would have with flux core wire...
FWIW the flow rat is a bit more important than pressure, the pressure simply means you have gas present.
Have you double checked the polarity? Your work should be negative (-) and the electrode positive (+) for gas and reverse for flux core...
Sounds to me like your close..
Please understand that I am trying to help you improve your skills, not criticize, it takes a lot of courage to try something new and when I was learning to weld I needed a lot of encouragement.
Great job